Hi I have a 3608 I've noticed on my decks they appear to be yellow in appearance is this due to poor gel coat showing the resin through or is there an easy fix as it bugs me to see it. Regards lee
- waybomb
- CYO Moderator

- Posts: 2745
- Joined: February 5th, 2013, 9:24 pm
- Vessel Info: 1995 Boston Whaler Rage15
1987 3697 Carver Mariner
1988 Cougar 46 Kevlar Vee offshore
1969 15' Glasspar / 1967 Johnson Electromatic 85 - Location: Saint Joseph,Mi
- Has thanked: 69 times
- Been thanked: 492 times
Re: decks
We use soft scrub for most stains. The stain may be iron left from evaporated water. A mild acid will dissolve the rust.
Thanks
Fred
1969 Glaspar Avalon /1967 Johnson Electromatic 85
1987 Carver Mariner
1988 Cougar Kevlar 46' with triple blown 572 ci
1995 Boston Whaler Rage
Past - 1988 2807, 1989 4207 Aft
Fred
1969 Glaspar Avalon /1967 Johnson Electromatic 85
1987 Carver Mariner
1988 Cougar Kevlar 46' with triple blown 572 ci
1995 Boston Whaler Rage
Past - 1988 2807, 1989 4207 Aft